Information Journal Paper
APA:
Copy. (2017). Effect of the manual (GMAW) and pulsed (P-GMAW) welding processes on impact strength and fracture behavior of AISI 304-AISI 1040 dissimilar steel joints fabricated by ASP316L austenitic stainless steel filler metal. KOVOVE MATERIALY METALLIC MATERIALS, 55(2), 141-148. SID. https://sid.ir/paper/786195/en
Vancouver:
Copy. Effect of the manual (GMAW) and pulsed (P-GMAW) welding processes on impact strength and fracture behavior of AISI 304-AISI 1040 dissimilar steel joints fabricated by ASP316L austenitic stainless steel filler metal. KOVOVE MATERIALY METALLIC MATERIALS[Internet]. 2017;55(2):141-148. Available from: https://sid.ir/paper/786195/en
IEEE:
Copy, “Effect of the manual (GMAW) and pulsed (P-GMAW) welding processes on impact strength and fracture behavior of AISI 304-AISI 1040 dissimilar steel joints fabricated by ASP316L austenitic stainless steel filler metal,” KOVOVE MATERIALY METALLIC MATERIALS, vol. 55, no. 2, pp. 141–148, 2017, [Online]. Available: https://sid.ir/paper/786195/en