مرکز اطلاعات علمی Scientific Information Database (SID) - Trusted Source for Research and Academic Resources

Persian Verion

Scientific Information Database (SID) - Trusted Source for Research and Academic Resources

video

Scientific Information Database (SID) - Trusted Source for Research and Academic Resources

sound

Scientific Information Database (SID) - Trusted Source for Research and Academic Resources

Persian Version

Scientific Information Database (SID) - Trusted Source for Research and Academic Resources

View:

1,350
Scientific Information Database (SID) - Trusted Source for Research and Academic Resources

Download:

0
Scientific Information Database (SID) - Trusted Source for Research and Academic Resources

Cites:

Information Journal Paper

Title

Preparation and comparison of natural and synthetic hydroxyapatite scaffolds made by cold isostatic pressing method

Pages

  113-124

Abstract

 Due to its bioactivity and biocompatibility properties, hydroxyapatite (HA) with Ca10(PO4)6OH2 chemical formula has been broadly employed for bone and teeth treatment applications as hard tissue. In the present research, hydroxyapatite was synthesizedvia sol-gel and natural (extraction from bovine cortical bone) methods. Natural hydroxyapatite had an average particle size of about 5 μ m and synthetic hydroxyapatite powders wereless than100 nm. Therefore, synthetic hydroxyapatite powders size was smaller than natural hydroxyapatite powders. Scaffolds were prepared by cold isostatic pressing method (CIP) and sintered at 1300° C. In order to evaluate the characteristics of the produced hydroxyapatite and morphological investigation, X-ray diffraction (XRD) and Fourier Transform infra-red spectroscopy (FTIR) were performed on the samples. Scanning electron microcopy (SEM) and Atomic force microscopy (AFM) were carried out to investigate the particle size, size and morphology of porosities and to study thetopography of surfaces. The results of scanning electron microscopy were in agreement with the AFM topography. After measuring the density of scaffolds, the compression tests were carried out on standard samples. Accordingly, the compression strength and density of samples from synthetic hydroxy apatite were more than those of the samples produced from natural hydroxyapatite. The compression strength of synthetic hydroxyapatite scaffold was 55. 6 MPa and its density was 2. 97 g/cm3. Cell culture was done on hydroxyapatite scaffolds with human osteoblast stem cells after14 days. Results showed that cell proliferation on natural hydroxyapatite scaffolds were less than synthetic hydroxyapatite scaffolds.

Cites

  • No record.
  • References

    Cite

    APA: Copy

    HEIDARI, FATEMEH. (2018). Preparation and comparison of natural and synthetic hydroxyapatite scaffolds made by cold isostatic pressing method. JOURNAL OF NEW MATERIALS, 9(1 (33) ), 113-124. SID. https://sid.ir/paper/169781/en

    Vancouver: Copy

    HEIDARI FATEMEH. Preparation and comparison of natural and synthetic hydroxyapatite scaffolds made by cold isostatic pressing method. JOURNAL OF NEW MATERIALS[Internet]. 2018;9(1 (33) ):113-124. Available from: https://sid.ir/paper/169781/en

    IEEE: Copy

    FATEMEH HEIDARI, “Preparation and comparison of natural and synthetic hydroxyapatite scaffolds made by cold isostatic pressing method,” JOURNAL OF NEW MATERIALS, vol. 9, no. 1 (33) , pp. 113–124, 2018, [Online]. Available: https://sid.ir/paper/169781/en

    Related Journal Papers

    Related Seminar Papers

  • No record.
  • Related Plans

  • No record.
  • Recommended Workshops






    Move to top